STI liner oxidation removes silicon damage and rounds trench corners to reduce electric field crowding and prevent parasitic channels [P2].
STI liner oxidation is positioned immediately after the liner pre-clean and before any conformal liner deposition because it directly defines the silicon–oxide interface quality at the trench sidewall and bottom, which is a dominant determinant of isolation reliability and stress coupling into adjacent active regio…
Read the full explanation and sources for free.