In vertically stacked nanosheet gate-all-around (GAA) transistors, the inner spacer isolates the replacement metal gate from epitaxial source/drain regions while locking in effective gate length through selective lateral SiGe cavity etching . Because inner-spacer thickness reduces gate-to-source/drain fringe capacitance at the cost of higher extension resistance and altered bottom punch-through-stopper coupling, cavity rectangularity and seam-free conformal fill directly govern switching speed and leakage .
Why GAA Nanosheets Need Inner Spacers Beyond FinFET Sidewall Spacers
As logic scaling reaches the physical gate-pitch and electrostatic boundaries of tri-gate FinFETs, vertically stacked silicon nanosheet GAAFETs regain wrap-around gate control across stacked horizontal channels , building upon concepts in planar, FinFET, and GAA transistor structures. Unlike FinFETs—where conventional exterior spacers documented in sidewall spacer fundamentals and the 14nm sidewall spacer flow flank a continuous vertical fin—a GAA superlattice interleave alternates sacrificial SiGe and channel Si layers under the dummy gate .
If source/drain cavities were simply etched vertically and refilled without indenting and plugging the exposed SiGe layer ends, subsequent selective Si and SiGe epitaxy would merge directly against the sacrificial layers, leaving no dielectric barrier to separate epitaxial source/drain regions from the later replacement metal gate . Conversely, without an intact inner spacer, the isotropic channel-release etch that removes sacrificial SiGe beneath the gate would attack and undermine the grown source/drain epitaxy .
7nm FinFET
Use the 7nm FinFET flow overview to compare conventional outer sidewall spacers against sub-5nm GAA inner-spacer integration; courses cover 40nm-7nm.
Open 2.5D flow map, module handoffs & public cross-sections.
Lateral SiGe Cavity Etch Regimes and Profile Control
Forming each inner-spacer cavity requires laterally recessing SiGe layers inside the source/drain trench with extreme etching selectivity over the adjacent Si nanosheets and dielectric hardmasks . Comparative dry-etching studies distinguish three major process regimes :
- Inductively coupled plasma (ICP): Directional physical ion sputtering severely narrows the SiGe-to-Si selectivity window and erodes exposed Si nanosheet ends into rounded tips .
- Remote plasma etching (RPS): Suppressing direct ion bombardment improves silicon preservation, yet isotropic reactive radicals aggressively consume silicon oxide and nitride hardmasks or outer spacers .
- Thermal gas etching: Purely thermally activated gas-phase etching relies on activation-energy differences between SiGe and Si to achieve superior selectivity and flat sheet ends .
Even under thermal gas etching, achieving uniform cavity profiles across top, middle, and bottom nanosheets demands two kinetic safeguards: thorough removal of native oxide or etch-blocking polymers prior to recess, and balanced thermal and pressure control . Raising reactant supply pressure transitions the process out of mass-transport starvation—which causes crescent-shaped sidewall curvature and shallower bottom-layer cavities—into a surface-reaction and byproduct-desorption rate-limiting regime that yields flat, rectangular cavities . Sheet-resolved metrology remains essential because lateral indentation depth responds sensitively to superlattice Ge composition and individual layer thickness .
Conformal Dielectric Fill, Pull-Back Anisotropy, and Pinch-Off Seams
Once rectangular SiGe cavities are formed, filling high-aspect-ratio recessed pockets and stripping excess outer dielectric imposes coupled deposition and etch constraints . Poorly conformal plasma-enhanced CVD easily pinches off at the narrow cavity mouth, whereas high-conformality LPCVD or atomic-layer low- films fill deep pockets smoothly . During subsequent dielectric pull-back, the etch must clear vertical outer spacer walls and every Si nanosheet tip completely without leaving nitride residue on the crystalline Si seed facets required for defect-free S/D epitaxy, yet avoid over-etching back into the cavity .
Intriguingly, seam engineering is not binary . When a small air-gap seam forms completely sealed inside the interior of the inner spacer, it lowers the effective dielectric constant and decreases parasitic gate-to-source/drain capacitance . By contrast, an open pinch-off seam exposed at the outer cavity face degrades epitaxial seed nucleation and introduces reliability hazards .
Parasitic Capacitance, Extension Resistance, and Bottom PTS Sensitivity
Inner-spacer lateral thickness sets a multi-variable electrical tradeoff linking gate-to-S/D capacitance, channel length, and source/drain resistance :
Thickening pushes the replacement metal gate farther away from doped epitaxial source/drain blocks, curbing fringing parasitic capacitance . However, excessively deep indentation shortens the active gate length , lengthens the high-resistivity semiconductor extension path under the spacer, raises extension resistance , and reduces drive current; meanwhile, an overly thin spacer risks structural breach during SiGe channel release .
Device-level sensitivity analysis also reveals a sharp vertical asymmetry across stacked sheets . Top and middle inner spacers sit symmetrically between two Si nanosheet channels, whereas the bottom inner spacer borders only one bottom Si sheet above the bulk punch-through stopper (PTS) substrate . When S/D trench over-etch deepens and fast-diffusing NFET S/D dopants (such as phosphorus) penetrate near the sub-fin boundary, the PTS potential barrier drops—making NFET off-state leakage (short-channel DIBL) and PFET drive current acutely sensitive to bottom inner-spacer thickness variation .
Connecting GAA Inner Spacer Physics to 40nm-7nm Course Flows
To compare conventional exterior sidewall spacers, selective S/D epitaxy, and replacement metal gate flows that precede stacked-nanosheet inner-spacer integration, inspect the 7nm FinFET flow overview. Interactive 2.5D courses cover 40nm-7nm planar and FinFET nodes; 3nm and sub-3nm GAA inner-spacer cavity formation lies beyond the interactive course curriculum.
Continue along the process chain
Follow what precedes and follows this concept in a real wafer flow — open interactive cross-sections with zero paywall dead ends.
Transfer Oxide Deposition
Inspect Step #5 (STI) in the 7nm flow with interactive 2.5D cross-section.
Fin Recess Etch
Inspect Step #93 (STI) in the 7nm flow with interactive 2.5D cross-section.
Spacer etch-back: coating, removal and retention
Mark film for removal or retention, predict the etched profile, then apply your reasoning to a trench.
References
Meng Wang, Xinlong Guo, Ziqiang Huang et al., "Feature Comparison and Process Optimization of Multiple Dry Etching Techniques Applied in Inner Spacer Cavity Formation of GAA NSFET," Nanomaterials, 2026.
Sanguk Lee, Jinsu Jeong, Jun-Sik Yoon et al., "Sensitivity of Inner Spacer Thickness Variations for Sub-3-nm Node Silicon Nanosheet Field-Effect Transistors," Nanomaterials, 2022.
Junjie Li, Yongliang Li, N. Zhou et al., "Study of Silicon Nitride Inner Spacer Formation in Process of Gate-all-around Nano-Transistors," Nanomaterials, 2020.
D. Schmidt, A. Cepler, C. Durfee et al., "Development of SiGe Indentation Process Control for Gate-All-Around FET Technology Enablement," IEEE transactions on semiconductor manufacturing, 2022.
Qingzhu Zhang, Yongkui Zhang, Yan-Na Luo et al., "New structure transistors for advanced technology node CMOS ICs," National Science Review, 2024.